Cold rolled steel plate and coil are produced by re-rolling hot rolled, pickled substrate at room temperature. That additional pass delivers tighter thickness and width tolerances, a smoother surface and better flatness than hot rolled product, while the low carbon content and controlled annealing keep elongation high enough for severe forming work. The result is a forming-quality material used for stamping, drawing, bending, welding and as substrate for metallic and organic coatings.
Grade Range and How It Is Organised
The DC series is defined in EN 10130, the European standard for cold rolled low carbon steel flat products for cold forming. Grades are ranked by forming severity rather than by strength: DC01 is the basic forming grade, DC03 to DC05 cover progressively deeper drawing, and DC06 is the ultra deep drawing grade. DC02 appeared in older editions of the standard and is rarely specified today, while DC07 sits above DC06 for extreme forming. Supplying the whole DC01 to DC06 range from one source lets a fabricator match each component to the lowest grade that forms reliably, instead of over-specifying deep drawing quality on simple parts.
Grade Selection by Forming Severity
Selection starts from the shape of the part: how deep it must be drawn, how sharp the radii are, and how visible the surface will be.
| Grade | Forming capability | Typical parts |
|---|---|---|
| DC01 | Standard forming, bending and light stamping | Sheet metal housings, brackets, simple embossed panels |
| DC03 | Light to moderate drawing and forming | Mild stampings, simple enclosures, flat panels |
| DC04 | Deep drawing and press forming of moderately complex shapes | Appliance shells, structural light parts |
| DC05 | Good deep draw performance with reduced springback | Deeper drawn parts that need extra ductility |
| DC06 | Extra deep drawing for the largest deformation | Automotive body panels, fuel tanks, deep appliance shells |
Mechanical Requirements That Decide Forming Success
EN 10130 controls the properties that decide whether a press shop can run a part without splitting or wrinkling: yield strength for forming load, tensile strength for strength assessment, elongation for ductility, the plastic strain ratio r90 for resistance to thinning in the drawn wall, and the work hardening exponent n90 for the way strain spreads through the part. The values below reflect the ranges normally met in production for each grade.
| Grade | Re MPa | Rm MPa | A80 min % | r90 min | n90 min |
|---|---|---|---|---|---|
| DC01 | 140 - 280 | 270 - 410 | ≥ 28 | - | - |
| DC03 | 140 - 240 | 270 - 370 | ≥ 34 | ≥ 1.3 | - |
| DC04 | 140 - 210 | 270 - 350 | ≥ 38 | ≥ 1.6 | ≥ 0.18 |
| DC05 | 140 - 180 | 270 - 330 | ≥ 40 | ≥ 1.9 | ≥ 0.20 |
| DC06 | 120 - 170 | 270 - 330 | ≥ 41 | ≥ 2.1 | ≥ 0.22 |
Surface Finishes and Processing Conditions
Surface and processing condition are agreed with the forming grade, because the same grade can be supplied in several finishes for different downstream routes.
Dry finish - for parts that are welded or coated later and do not need immediate protection.
Oiled - a light film that limits oxidation during storage and transport.
Skin passed - a light final reduction that improves flatness and surface consistency for visible parts.
Annealed - lower hardness and higher elongation for the deepest drawing operations.
Matte or bright finish - chosen to match the painting and appearance requirements of external panels.
Equivalent Grades, Tolerances and Quality Control
Because the DC series is used worldwide, equivalent designations help importers and designers cross-check drawings. DC01 corresponds to JIS SPCC and to the ASTM CS Type A designation, DC03 and DC04 correspond broadly to JIS SPCD and SPCEN, and the higher drawing grades are compared with the ASTM DS and DDS type grades. Thickness and width tolerances follow the applicable part of the product standard for the ordered condition and size, and flatness and surface quality are agreed for visible classes of part. Batch-to-batch consistency is the practical quality target for high volume users: stable yield strength keeps press settings unchanged, and uniform r90 and n90 values keep draw depth repeatable. Coils and sheets are checked for thickness profile, surface condition, mechanical properties and, on coated material, coating adhesion before dispatch.
FAQ
Q: What is the difference between cold rolled and hot rolled steel?
Cold rolled steel is hot rolled coil that has been pickled and re-rolled at room temperature. It offers closer tolerances, a smoother surface and better formability, while hot rolled product is usually less costly and available in heavier thicknesses.
Q: Which DC grade suits a deep drawn part?
Start from the drawing ratio and the complexity of the shape. DC04 covers most ordinary deep draws, DC05 suits deeper parts with a tight limit on wall thinning, and DC06 is reserved for large deformation where the risk of cracking is highest.
Q: Is DC02 still available?
DC02 was listed in older editions of EN 10130 and has since been withdrawn. DC01 is used for simple forming and DC03 for light drawing in current specifications.
Q: What does the r90 value tell a press shop?
The plastic strain ratio r90 measures resistance to thickness reduction in the plane of the sheet. A higher value means the wall of a drawn part thins less, so deeper draws can be produced at the same starting thickness.
Q: Can cold rolled sheet be supplied with a zinc coating?
Yes. Cold rolled substrate is the normal basis for hot dip zinc coated grades, so the forming grades described here are also available as coated product when corrosion protection is required together with drawability.
Q: How is thickness tolerance controlled?
Thickness tolerance is agreed against the applicable product standard for the grade, condition and size that are ordered, and it is verified along the coil during production rather than at a single point.