S350gd Steel
S350gd is a grade in the European standard "EN 10346-2009 Continuous Hot-Dip Galvanized Steel Sheet Products", which is a galvanized steel sheet. S350G is structural steel requiring tensile strength greater than 350MPa, D means galvanized sheet, so s350gd is structural galvanized sheet with yield strength greater than 350MPa.
The S350G is available in the following hot dip coatings: S350GD+Z (galvanized), S350GD+ZF (galvanized-iron), S350GD+ZA (galvanized-aluminum), S350GD+AZ (aluminum-zinc), S350GD+AS (galvanized-iron) aluminum silicon).
Struggling to find S350GD Galvanized Steel with customized width and length? Unlike standard suppliers, GNEE STEEL specializes in OEM customization. We can produce coils and sheets in your exact dimensions, with minimum order quantities as low as 5 tons. Read on to explore our customization cases and strict quality control process.

S350GD Galvanized Steel
Specifications Table
| Quality | Standard | Material No. | Available coatings |
|---|---|---|---|
| S350GD | DIN EN 10346 | 1.0529 | +Z, +ZF, +ZA, +ZM, +AZ, +AS |
| Testing direction | Yield strengthRP02 (MPa) |
Tensil Strength Rm (MPa) |
Elongation A80 (in %) |
|---|---|---|---|
| L | ≥ 350 | ≥ 420 | ≥ 16 |
| C % |
Si % |
Mn % |
P % |
S % |
|---|---|---|---|---|
| ≤ 0,20 | ≤ 0,60 | ≤ 1,70 | ≤ 0,10 | ≤ 0,045 |
Properties
S350GD combines high strength with excellent ductility and long-lasting corrosion protection. The most important key mechanical values can be found in the table above.
These characteristic values enable reliable load-bearing capacity even under dynamic or impact loads. The hot-dip galvanized surface (+Z) offers solid basic corrosion protection. Due to the variants
+Z (pure galvanized):
Standard corrosion protection for general conditions.
+ZF (zinc-iron):
Improved coating adhesion and increased resistance to mechanical stress.
+ZA (zinc-aluminium):
Optimized resistance in atmospheric environments.
+ZM (zinc-magnesium):
Extended protection in maritime and saline zones through passivating behavior.
+AZ (aluminum-zinc):
Combination of heat resistance and corrosion protection, ideal for high surface temperatures.
+AS (aluminum-silicon):
Especially for applications with extreme temperature influences and high corrosion loads.
can also be used to create customized protection profiles. For example, +ZF increases the adhesion of the zinc coating, +ZA and +ZM improve corrosion resistance in industrial and maritime atmospheres respectively, +AZ combines heat resistance with corrosion protection, and +AS offers maximum protection at high temperatures or in chemically aggressive environments. In addition, S350GD has a homogeneous microstructure, good weldability and excellent dimensional stability, which ensures precise further processing in cutting, bending and welding processes.
Corrosion Resistance
| Corrosive Agent | Concentration (%) | Temperature (°C) | Resistance Rating | Notes |
|---|---|---|---|---|
| Chlorides | 3% | 25 °C | Fair | Risk of pitting |
| Sulfuric Acid | 10% | 20 °C | Poor | Not recommended |
| Sodium Hydroxide | 5% | 25 °C | Good | Limited exposure acceptable |
S350GD steel demonstrates good resistance to atmospheric corrosion and moderate resistance to chlorides. However, it is susceptible to corrosion in acidic environments, which can lead to rapid degradation. Compared to other grades like S235 and S355, S350GD offers superior corrosion resistance due to its galvanization, making it a preferred choice in environments prone to moisture and corrosive agents.
- Available Steel Grade
|
Standard |
Grade |
C |
Si |
Mn |
P |
S |
Ti |
|
Forcold Forming Chinese Standard |
DX51D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
DX52D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
|
DX53D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
|
DX54D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
|
DX56D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
|
DX57D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
|
Forcold Forming Japanese Standard |
SGCC |
0.15 |
0.50 |
0.80 |
0.050 |
0.030 |
0.025 |
|
SGCD1 |
0.12 |
0.50 |
0.60 |
0.040 |
0.030 |
0.025 |
|
|
SGCD3 |
0.08 |
0.50 |
0.45 |
0.030 |
0.030 |
0.025 |
|
|
SGCD4 |
0.06 |
0.50 |
0.45 |
0.030 |
0.030 |
0.025 |
|
|
For Structure Japanese Standard |
SGC340 |
0.25 |
0.50 |
1.70 |
0.200 |
0.035 |
0.025 |
|
SGC400 |
0.25 |
0.50 |
1.70 |
0.200 |
0.035 |
0.150 |
|
|
SGC490 |
0.30 |
0.50 |
2.00 |
0.200 |
0.035 |
0.025 |
|
|
SGC510 |
0.30 |
0.50 |
2.50 |
0.200 |
0.035 |
0.025 |
|
|
For Structure AISI Standard |
S220GD+Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.025 |
|
S250GD+Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.025 |
|
|
S280GD+Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.025 |
|
|
S320GD+Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.025 |
|
|
S350GD+Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.150 |
|
|
S550GD+Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.150 |
Unlike ordinary galvanized steel, the precise matching of yield strength and coating thickness in S350GD galvanized steel ensures stable performance in high wind pressure and high corrosion environments. If you are facing material selection confusion or need to compare performance differences between different grades of galvanized steel, please feel free to contact us for one-on-one consulting services at any time.
Contact us for the latest
S350GD galvanized steel price and technical datasheet.