DC03 1.0347 Steel

Jan 19, 2024

DC03 ( 1.0347 )

Grade : DC03
Number: 1.0347
Classification: Non-alloy quality steel
Standard:
EN 10130: 2006 Cold rolled low carbon steel flat products for cold forming. Technical delivery conditions
EN 10139: 1997 Cold rolled uncoated mild steel narrow strip for cold forming. Technical delivery conditions
EN 10152: 2009 Electrolytically zinc coated cold rolled steel flat products for cold forming. Technical delivery conditions
EN 10271: 1999 Electrolytically zinc-nickel (ZN) coated steel flat products. Technical delivery conditions
Equivalent grades: Go here

 

dc03 steel
 

Chemical composition % of steel DC03 (1.0347): EN 10130-2006

Unless otherwise agreed at the time of enquery and order, this grade may be supplied as alloy steel (for example with boron or titanium)
C Mn P S
max 0.1 max 0.45 max 0.035 max 0.035

dc03 1.0347
 

Mechanical properties of steel DC03 (1.0347)

Rm - Tensile strength (MPa) 270-370

 

ReH - Minimum yield strength (MPa) 240

 

A - Min. elongation Lo = 80 mm (%) 34

 

A - Min. elongation Lo = 5,65 √ So (%) (+A) 37

 

Vickers hardness ( HV): (+A) 100


Equivalent grades of steel DC03 (1.0347)

Warning! Only for reference

EU
EN
Germany
DIN,WNr
Japan
JIS
France
AFNOR
England
BS
European old
EN
Italy
UNI
Spain
UNE
Sweden
SS
Czechia
CSN
Russia
GOST
DC03
1.0336
St13
USt14
SPCD
E
CR2
CR3
FeP03
FeP02
AP02
1146
11304
08YU


Mechanical properties

ReH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d elasticite minimale
Rm Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc


Heat treatment conditions

+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated

 

Non-alloy quality steel
Chemical composition of steel DC03 (1.0347), Standards of steel DC03 (1.0347)
Mechanical Properties of steel DC03 (1.0347) Equivalent grades of steel DC03 (1.0347)
steel DC03 (1.0347) Tensile Strength, Elongation, Proof strength , Hardness