Where DS Sits in ASTM A1008
ASTM A1008 covers cold rolled carbon steel sheet and strip, and organises the grades by forming severity. Commercial Steel, or CS, is the baseline for parts that are bent or lightly formed. Drawing Steel, or DS, is one step above it and is intended for parts that are formed in a press, with better ductility and tighter chemistry control than CS. Above DS are Deep Drawing Steel, DDS, and Extra Deep Drawing Steel, EDDS, which target the most severe draws. Within the DS class, ASTM A1008 defines three sub-types, A, B and C, that differ in their guaranteed mechanical range and in the restrictions placed on carbon, manganese and phosphorus.
Sub-Type Comparison
| Characteristic | DS Type A | DS Type B | DS Type C |
|---|---|---|---|
| Main objective | Basic press forming | Standard drawing performance | Higher drawing performance |
| Strength and hardness | Relatively high | Medium | Relatively low |
| Formability | Basic level | Common level | Better |
| Chemistry control | Relatively loose | Moderate | Stricter |
| Phosphorus, P | 0.025 % max. | 0.025 % max. | 0.020 % max. |
| Typical parts | Simple stampings, brackets, tool boxes | Electrical housings, panels, containers | Deeper shapes, fuel tanks, lamp housings |
The phosphorus limit is the clearest dividing line. Phosphorus strengthens ferrite by solid solution and raises the transition temperature, so a tighter ceiling is used whenever the part must survive a deep draw without cracking in cold conditions. DS Type C holds P to 0.020 percent maximum for this reason, while Type A accepts the highest strength and the lowest cost of the three. In practice, tabulated mill values for DS grades sit in a tensile range of roughly 270 to 400 MPa, with Type C at the ductile end of the band and elongation minimums in the low thirties and above.
Equivalents in Other Standards
DS Type B, the most widely ordered sub-type, is normally compared with the EN 10130 drawing grade DC03 and the JIS G3141 drawing quality grade SPCD, with DC04 and SPCE relevant when the draw is deeper. DS Type C approaches the Japanese DDS class and the European DC04 to DC05 range. These mappings are commercial conventions rather than exact identities, because each standard defines its own test methods, tolerances and acceptance rules, so substitution should always be confirmed by comparing the guaranteed tensile, elongation and chemistry values clause by clause.
Processing Notes for Press Shops
Confirm whether the part needs guaranteed formability or only nominal ductility; the difference between Type A and Type C is measurable in tool load and scrap rate.
Keep punch and die clearances at about 8 to 12 percent of thickness per side for these mild steels, and reduce clearance for fine blanking.
Use a lubricant matched to draw depth; the smooth, low roughness surface of skin passed cold rolled stock holds oil well but drains it quickly from vertical walls.
Check coil set and crossbow before blanking, since flatness deviation consumes drawing allowance at the blank edge.
For welded assemblies, the low carbon content gives a soft, crack resistant weld zone, so spot and laser welding behave predictably.
Quality Control and Documentation
Cold rolled drawing steel is normally supplied skin passed and oiled with surface quality agreed to the ASTM A1008 surface condition classes, from general purpose to exposed part quality. Thickness tolerance follows the standard tables and should be quoted with the order, since half tolerance practice materially changes cost. Mechanical testing covers tensile strength, yield strength and elongation to ASTM A370 methods, with r and n values measured where the drawing operation requires them. Inspection documents to EN 10204 type 3.1, or a mill certificate of analysis for ASTM orders, together with a declared surface condition and oil type, form the usual evidence package for export shipments.
Frequently Asked Questions
Q: What does DS stand for in ASTM A1008?
A: Drawing Steel, the grade class intended for parts that are formed in a press rather than only bent.
Q: Which DS sub-type is used most often?
A: DS Type B, because it balances forming performance with a cost that suits the majority of stamped parts.
Q: When should DDS be selected instead of DS?
A: When the draw is too deep for DS Type C, specifically where the part requires significant wall thinning control or successive redrawing.
Q: Is DS Type C the same as DC04?
A: They occupy a similar position in their respective standards, but the guaranteed values differ, so a direct substitution should be verified from the certificate.
Q: Why is phosphorus limited in DS steel?
A: Phosphorus raises strength but reduces ductility and toughness, so a tight ceiling protects the part against cracking during cold forming.