What Surface Galvanizing Does for Steel Sheet
Surface galvanizing protects steel sheet with a zinc coating that corrodes preferentially to the steel beneath it, so the sheet keeps its load carrying section long after an uncoated surface would have started to rust. The dominant industrial method is hot-dip galvanizing, in which cleaned and fluxed steel is immersed in molten zinc and withdrawn so that a zinc-iron alloy layer and a pure zinc layer form metallurgically on the surface. The same principle serves two rather different products: continuous coil lines that coat strip at high speed for building, appliance and automotive sheet, and batch lines that coat cut and fabricated parts such as poles, frames and structural components. Electro-galvanizing, by contrast, deposits zinc electrolytically and produces a much thinner, smoother coating.
Stages of the Hot-Dip Galvanizing Line
The process is only as good as the surface preparation that precedes the zinc bath. Each stage has a defined purpose and a defined control point:
| Stage | Purpose | Typical Control |
|---|---|---|
| Alkali cleaning | Removes oil, grease and rolling emulsion from the strip or part | Bath concentration, temperature, contact time, rinse quality |
| Pickling | Dissolves mill scale and rust so that zinc can react with clean iron | Acid concentration, inhibitor, temperature, iron content of the bath |
| Rinsing and fluxing | Removes residual acid and applies a flux that lets molten zinc wet the surface | Rinse water cleanliness, flux density and drying before the bath |
| Zinc immersion | Forms the zinc-iron alloy layer and the outer zinc layer | Bath temperature of about 450-470 C, aluminium content, immersion time |
| Coating weight control | Sets the final coating mass on continuous lines | Gas wiping pressure and line speed for the target designation |
| Cooling and finishing | Solidifies the coating, levels the strip and prepares the surface | Cooling rate, skin pass or tension levelling, passivation and oiling |
On continuous lines the coil is coated, cooled, skin passed, passivated and oiled in one pass, so the surface condition delivered to the customer is fixed by the line settings rather than by any later operation. On batch lines the same sequence is applied to individual parts, and the coating mass is controlled by drainage and by the immersion time in the bath rather than by gas wiping.
Hot-Dip Continuous, Hot-Dip Batch and Electro-Galvanizing
Coating designation and coating mass are the practical differences between the products, and they determine where each one is used. Continuous hot-dip coatings are designated under EN 10346 by a letter that identifies the coating type and a number that gives the total coating mass in grams per square metre, both sides included. A Z100 coating therefore carries about 100 g/m2 of zinc in total, which corresponds to roughly 7 um per side, while a Z600 coating carries about 600 g/m2 in total, provided as equal or differential coating masses on the two sides where the order specifies it.
Hot-dip continuous: coating designations from about Z100 to Z600, with alloy coatings such as zinc-aluminium and aluminium-zinc for roofing, cladding and automotive sheet. Supplied as coil and cut sheet with a uniform, formable coating.
Hot-dip batch: coating thickness typically in the range of 45 um to over 100 um on fabricated parts, poles and frames, in accordance with EN ISO 1461 or ASTM A123/A123M.
Electro-galvanizing: a thin, smooth coating of a few micrometres, produced on continuously electroplated strip for painted panels and for applications needing precise, uniform coating weight and a fine surface.
Selection is driven by the environment and the design life. Where coating durability in an outdoor or industrial atmosphere dominates, hot-dip continuous or batch product is used and the coating mass is matched to the corrosivity category of the site. Where the surface will be painted and appearance or forming quality dominates, electro-galvanized or galvannealed sheet is usually preferred.
Coating Structure, Appearance and Verification
The hot-dip coating consists of zinc-iron alloy layers adjacent to the steel, topped by a pure zinc layer. The alloy layers give a hard, tightly bonded interface, while the outer zinc provides the sacrificial protection. The surface may show the characteristic spangle pattern, which is a normal feature of the solidification of the zinc and not a defect; a smooth, spangle-free finish is obtained by suppressing spangle growth during solidification. Coating adhesion is verified by bend tests on representative samples, in which the coating must remain sound and must not flake away from the steel at the bend radius specified for the product. Coating mass or thickness is verified gravimetrically by the stripping method or non-destructively with a magnetic gauge, at the number of positions required by the applicable standard, and the surface treatment, dimensions and mechanical properties are checked against the same standard before the coil or part is released.
Design practice matters as much as inspection. The coating is ductile, but a very sharp bend concentrates strain at the outer fibre and can crack a thick coating, so bend radii and forming schedules are set with the coating mass in mind. Cut edges expose steel and are normally protected by the sacrificial action of the adjacent coating, or by a repair coating where the edge will be exposed for a long service period.
Frequently Asked Questions
Q: What is the difference between hot-dip and electro-galvanized sheet?
Hot-dip sheet is immersed in molten zinc and carries a thick coating with zinc-iron alloy layers, suited to outdoor and structural use. Electro-galvanizing deposits zinc electrolytically to give a thin, very smooth coating for painted panels and for tight coating weight control.
Q: What does a coating designation such as Z100 mean?
Under EN 10346 the letter identifies the coating type and the number is the total coating mass in grams per square metre over both sides. Z100 is therefore about 50 g/m2 per side, equivalent to roughly 7 um of zinc per side.
Q: At what temperature does the zinc bath operate?
Continuous and batch hot-dip lines operate with a molten zinc bath in the range of about 450-470 C. The temperature, together with immersion time and bath chemistry, controls the thickness of the zinc-iron alloy layer.
Q: Is the spangle pattern on a galvanized surface a defect?
No. Spangle is a normal crystallisation feature of the zinc coating. It does not affect corrosion performance, and buyers who need a uniform appearance specify a spangle-free or minimum spangle finish instead.
Q: How is coating mass verified on a delivered coil?
Either gravimetrically, by dissolving the coating from a sample of known area, or non-destructively with a magnetic gauge calibrated for the coating. The number and location of readings, and the acceptance limits, are set by the standard referenced in the order.
Q: Can a hot-dip galvanized sheet be bent or deep drawn?
Yes. The coating is formable and is normally tested with a bend test. Sharp bends strain the coating heavily, so bend radii, die clearance and forming lubricants are selected with reference to the coating mass to avoid cracking or flaking.