| Class | Designation | Characteristics | Typical thickness (mm) | Typical width (mm) | Main applications |
|---|---|---|---|---|---|
| Commercial quality | SPCC / SPCCT | Suitable for bending and simple forming; the most widely used class | 0.18–3.0 | 600–1500 | Refrigerators, cabinets, distribution boards, drums |
| Drawing quality | SPCD | Drawing quality with excellent thickness uniformity | 0.18–2.0 | 600–1250 | Automotive floor and roof panels |
| Deep drawing quality | SPCE | Deep drawing quality with metallurgically controlled grain size; retains a good surface after deep drawing | 0.18–2.0 | 600–1250 | Automotive fenders and quarter panels |
| Extra deep drawing (non-aging) | SPCF | Non-aging steel for demanding deep drawing; resistance to stretcher-strain (fluting) over time | 0.18–2.0 | 600–1250 | Complex drawn automotive body parts |
| Super extra deep drawing | SPCG | Highest formability in the series for the most severe draws | 0.18–2.0 | 600–1250 | Severely drawn components with tight radii |
| Non-aging deep drawing | SPCEN | "N" suffix denotes guaranteed non-aging (strain-ageing free) performance | 0.18–2.0 | 600–1250 | Exposed auto panels requiring stable forming behaviour |
Thickness and width figures are typical available ranges from the supplier; the governing standard for grade and mechanical requirements is JIS G 3141 (current edition).
2. How the Grades Differ in Practice
All of these grades are low-carbon cold-rolled steels; the difference lies in how the steel is controlled during production. Higher formability classes receive tighter control of chemistry (lower carbon and residual elements), a more refined grain structure and more consistent mechanical properties across the coil. In practice, this means:
- SPCC is the workhorse grade for bending, blanking and light forming where the drawing depth is modest.
- SPCD is specified where parts are drawn to moderate depth and uniform behaviour from coil to coil matters.
- SPCE is used for deep-drawn parts that must keep a clean, unmarked surface - its controlled grain size is what preserves the finish after severe forming.
- SPCF / SPCG are chosen for the most severe draws; SPCF additionally offers non-aging behaviour, avoiding stretcher-strain marks that can appear on aged sheet during deep drawing.
3. Electrolytic Zinc-Coated Variants (SECC, SECD, SECE)
Where the formed part needs a thin, uniform zinc layer on both sides - for corrosion resistance before painting, or for electrical applications such as chassis parts and brackets - electrolytic galvanized (EG) cold-rolled steel is used. These grades share the same formability ladder as the bare grades, with the "S" prefix replaced by "SE":
- SECC - electrolytic zinc-coated commercial quality;
- SECD - drawing quality;
- SECE - deep drawing quality.
The governing standard for the coating and base material is JIS G 3313 (current edition). Typical coating thicknesses are in the range of 5–20 µm per side, so SEC series corrosion protection is lighter than hot-dip galvanizing - it is a processing and painting aid rather than a heavy-duty barrier.
4. Surface Treatment Suffixes (Fingerprint-Resistant Coatings)
For appliance and electronic chassis applications, EGL sheet is often supplied with an added anti-fingerprint organic or inorganic coating. Common industry designations use a suffix after the grade (e.g. SECC-K2):
K2 - organic (resin-based) coating for fingerprint resistance and better paint adhesion;
KS - inorganic (silicate-based) coating;
CS-type - a UF-treated fingerprint-resistant finish designation used in some supply chains.
Coating designation systems vary by mill and market; always confirm the exact coating type, coating weight and lubricant status with the supplier in writing before ordering.
5. Selection Checklist for Mold and Die Designers
Estimate the draw ratio and forming severity; select SPCC → SPCD → SPCE → SPCF/SPCG as severity increases.
If the part is exposed and appearance matters, choose SPCE or better for grain-size control.
If parts are stored between rolling and forming, specify a non-aging grade (SPCF/SPCEN) to avoid fluting.
If corrosion resistance or paintability before assembly is required, consider the SEC series (JIS G 3313).
Always confirm mechanical property limits (yield, tensile, elongation), thickness tolerance and surface finish against the governing standard and the mill certificate.
Popular specifications are in short supply!
click to get the specification sheet!
| Classification | Designation | Characteristics | Size ( mm ) | Main applications |
| Commercial quality | SPCC,SPCCT | Commercial quality suitable for bending fabrication and simple forming; this is the type in greatest demand. | Thickness 0.18-3.0 Width 600-1500 |
Refrigerators, cabinets, power distribution boards and drums. |
| Drawing quality | SPCD | Drawing quality second only to that of SPCEN. Excellent uniformity. | Thickness 0.18-2.0 Width 600-1250 |
Automobile floor and roof panels. |
| Deep-drawing quality | SPCE,SPCF | Deep-drawing quality. With metallurgically controlled grain size, it retains its beautiful finish even after being deep-drawn. | Thickness 0.18-2.0 Width 600-1250 |
Automobile fenders and quarter panels |
Packaging and Shipping

GNEE STEEL specializes in cold-rolled steel sheets, galvanized steel coils, and galvanized steel pipes, offering a wide range of specifications in compliance with international standards such as ASTM, EN, JIS, and GB. Whether serving the construction, automotive, appliance, or infrastructure sectors, we offer the right steel solutions for your needs.