Cold Rolled Steel DC07 vs DC06

 

Many engineers and sourcing managers compare DC07 and DC06 during material selection for deep drawing. While both grades belong to the high-formability cold rolled steel family, their performance varies depending on the complexity of the final product. Understanding the differences helps factories reduce scrap rate and improve forming success.

 

DC06 provides highly reliable forming while offering low yield strength and good elongation. However, when forming geometry becomes extremely deep, curved or multi-stage, DC06 may not deliver the required stability. DC07, on the other hand, is specifically developed for "extreme forming limits", offering greater resistance to thinning and edge cracking.

 

Direct Property Comparison

 

Property DC06 DC07
Deep drawing capability ★★★★☆ ⭐⭐⭐⭐⭐
Risk of cracking Medium Very Low
Thickness uniformity High Very High
Suitable for Difficult shapes Extremely complex shapes

 

Practical recommendation

 

Application Best Choice
Automotive inner panels DC06
Fuel tanks / Cylinder casings DC07
Kitchen appliances housing DC06
High-precision industrial shells DC07

 

The super deep drawing grade DC07 is specified according to the standard DIN EN 10130, which focuses on cold-rolled flat products made of soft steels for cold forming. This standard ensures that the technical requirements and test methods for cold-rolled products are met, which are of great importance in various industrial applications, especially where the highest demands are placed on formability and surface quality.

 

DC07 is a particularly low-carbon steel characterized by exceptional cold formability. The chemical composition of DC07 is strictly controlled to ensure its excellent mechanical properties. The carbon content in DC07 is typically a maximum of 0.01 %, while the manganese content is a maximum of 0.20 %. The addition of micro-alloyed elements such as titanium and niobium can further improve formability and strength.

 

Quality Standard Material No.
DC07 DIN EN 10130 1.0898
DC07+ZE DIN EN 10152 1.0898

 

DIN EN Standard Testing direction Yield Point Re
(MPa)
Tensil Strength
Rm (MPa)
Elongation
A80 (in %)
r90 n90
10130 Q ≤ 150 250 – 310 ≥ 44 ≥ 2,5 ≥ 0,230
10152 Q ≤ 160 250 – 310 ≥ 43 ≥ 25 ≥ 0,220

 

To obtain high-quality DC07 and other cold rolled grades, GNEE STEEL supplies DC01, DC03, DC04, DC05, DC06 and DC07 with global shipping and professional technical support.

 